Steel forgings and rolled or forged bars for pressure purposes — Technical delivery conditions — Part 3: Nickel steels with specified low temperature properties
压力用钢锻件和轧制或锻造棒材——技术交付条件SPART 3:具有规定低温性能的镍钢
发布日期:
1999-07-08
1.1 ISO 9327的这一部分适用于制造的厚度不超过50毫米的锻件和轧制或锻造棒材
由表1中列出的钢材制成,并根据ISO 9327-1中给出的规格交付。
1.1 ISO 9327的这一部分涵盖以下数据:
a)在表1中,
根据铸件分析的化学成分;
室温下的拉伸性能;
交货时通常热处理条件的指示;
b)在表2中,对于铸造分析给出的极限值,允许的产品分析公差;
c)表3中的最小冲击能量值。
1.1 This part of ISO 9327 applies to forgings and rolled or forged bars in thicknesses up to 50 mm manufactured
from the steels listed in Table 1 and to be delivered according to the specifications given in ISO 9327-1.
1.1 This part of ISO 9327 covers the following data:
a) in Table 1 the limits for
the chemical composition according to the cast analysis;
the tensile properties at room temperature;
the indications on the usual heat treatment condition at the time of delivery;
b) in Table 2 the permissible product analysis tolerances on the limiting values given for the cast analysis;
c) in Table 3 the minimum impact energy values.