Urine-absorbing aids for incontinence — Test methods for characterizing polymer-based absorbent materials — Part 4: Determination of moisture content by mass loss upon heating
尿失禁吸尿器——聚合物基吸水材料特性的试验方法第4部分:加热质量损失法测定含水量
发布日期:
2001-12-06
ISO 17190的本部分规定了交联聚丙烯酸酯加热时质量损失的测定方法
(PA)水分含量在0%到5%之间(按质量计)的高吸水性粉末。方法是
精确到±0.1%以内。
一般来说,该方法预计适用于以下粉末状聚合物高吸水性材料:
在15°C至150°C的温度下自由流动。除水以外的物质,在该温度下易挥发
温度范围,会干扰。
This part of ISO 17190 specifies a method for determining the mass loss upon heating for cross-linked polyacrylate
(PA) superabsorbent powders with a moisture content ranging between 0 % and 5 % by mass. The method is
accurate to within ± 0,1 %.
In general, this method is expected to be applicable to powdered polymeric superabsorbent materials that are
free-flowing at temperatures between 15 °C and 150 °C. Substances other than water, that are volatile in this
temperature range, will interfere.