首页 馆藏资源 舆情信息 标准服务 科研活动 关于我们
现行 SAE AMS5393G
到馆提醒
收藏跟踪
购买正版
Alloy Iron Castings, Sand, Moderate Corrosion and Heat Resistant, 2.0Cr - 20Ni (2.4 - 2.8C), Stress Relieved 合金铸铁件 砂型 中度腐蚀和耐热 2.0Cr-20Ni(2.4-2.8C) 应力消除
发布日期: 2007-04-13
自2007年4月起,SAE航空航天材料部已宣布本规范“取消”,并已被ASTMD A 439取代。当参考已取消的SAE AMS 5393时,应满足最新版ASTM A 439的要求。通过这一行动,本文件仍将列在航空航天材料规范索引的数字部分,并指出其已被ASTMD A 439取代。
This specification has been declared "CANCELLED" by the Aerospace Materials Division, SAE, as of April 2007, and has been superseded by ASTMD A 439. The requirements of the latest issue of ASTM A 439 shall be fulfilled whenever reference is made to the cancelled SAE AMS 5393. By this action, this document will remain listed in the Numerical Section of the Index of Aerospace Material Specifications noting that it has been superseded by ASTMD A 439.
分类信息
关联关系
研制信息
相似标准/计划/法规
现行
SAE AMS5392M
Alloy Iron Castings, Sand, Moderate Corrosion and Heat Resistant, 2.1Cr - 15Ni - 6.5Cu (2.4 - 2.8C), as Cast
合金铸铁件 砂型 中等腐蚀和耐热 2.1Cr-15Ni-6.5Cu(2.4-2.8C) 铸态
2007-04-13
现行
SAE AMS5351G
Steel Castings, Sand, Corrosion and Moderate Heat Resistant 13Cr Normalized and Tempered (Stabilized: Apr 2017)
正火和回火的耐腐蚀和中等耐热13Cr钢铸件(稳定:2017年4月)
2017-04-04
现行
SAE AMS5394D
Alloy Iron Castings, Ductile, Sand, Corrosion and Heat Resistant, 2.0Cr - 20Ni (2.4 - 3.0C), Stress Relieved
耐腐蚀耐热球墨铸铁件 2.0Cr-20Ni(2.4-3.0C) 消除应力
2007-04-13
现行
SAE AMS5373E
Alloy Castings, Sand, Corrosion and Heat Resistant 16Co - 29Cr - 4.5W As Cast (Stabilized: Apr 2017)
耐腐蚀耐热合金铸件16Co-29Cr-4.5W铸态(稳定:2017年4月)
2017-04-06
现行
SAE AMS5395D
Alloy Iron Castings, Ductile, Sand, Corrosion Resistant 22Ni (2.5 - 3.0C) As Cast (Stabilized: Mar 2018)
耐腐蚀22Ni(2.5-3.0C)铸态球墨铸铁件(稳定:2018年3月)
2018-03-04
现行
SAE AMS4222H
Aluminum Alloy Castings, Sand, Moderate Heat Resistance 4.0Cu - 2.0Ni - 1.5Mg - 0.12Ti (242.0P) Solution Heat Treated and Stabilized (Stabilized: Apr 2017)
铝合金铸件 砂型 中等耐热性4.0Cu-2.0Ni-1.5Mg-0.12Ti(242.0P)固溶热处理和稳定化(稳定化:2017年4月)
2017-04-05
现行
SAE AMS5389D
Alloy Castings, Sand, Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated (Stabilized: Apr 2017)
经固溶热处理的耐腐蚀耐热合金铸件55Ni-16.5Cr-17Mo-4.5W-5.8Fe-0.40V(稳定:2017年4月)
2017-04-18