Copper, lead, zinc and nickel sulfide concentrates — Determination of arsenic — Part 1: Iron hydroxide concentration and inductively coupled plasma atomic emission spectrometric method
铜 铅 锌和硫化镍精矿砷的测定第1部分:氢氧化铁浓度和电感耦合等离子体原子发射光谱法
发布日期:
2014-10-30
ISO 13547-1:2014规定了一种测定铜、铅、锌和硫化镍精矿中砷质量分数的氢氧化铁浓度和电感耦合等离子体原子发射光谱法(ICP-AES)方法,如下所示:对于硫化铜精矿,该方法适用于测定0.05%至2.0%的砷质量分数;对于硫化铅精矿,该方法适用于砷的质量分数从0.05%到1.0%的测定;
对于硫化锌精矿,该方法适用于砷的质量分数从0.05%到0.6%的测定;对于硫化镍精矿,该方法适用于砷质量分数在0.05%至1.0%之间的测定。
ISO 13547-1:2014 specifies an iron hydroxide concentration and inductively coupled plasma atomic emission spectrometric (ICP-AES) method for the determination of the mass fraction of arsenic in copper, lead, zinc, and nickel sulfide concentrates as follows: for copper sulfide concentrates, the method is applicable to the determination of mass fractions of arsenic from 0,05 % to 2,0 %; for lead sulfide concentrates, the method is applicable to the determination of mass fractions of arsenic from 0,05 % to 1,0 %; for zinc sulfide concentrates, the method is applicable to the determination of mass fractions of arsenic from 0,05 % to 0,6 %; for nickel sulfide concentrates, the method is applicable to the determination of mass fraction of arsenic from 0,05 % to 1,0 %.