Carbonaceous materials for the production of aluminium — Anodes, cathodes blocks, sidewall blocks and baked ramming pastes — Determination of the thermal conductivity using a comparative method
铝生产用碳质材料——阳极、阴极块、侧壁块和烘烤捣打膏——用比较法测定导热系数
发布日期:
2004-07-08
ISO 12987:2004规定了在20°C至60°C温度范围内测定含碳材料导热系数的方法。这些材料的典型导热系数范围为2 W/(K·m)至100 W/(K·m)。
该方法可用于其他碳材料,例如用于其他应用的石墨化电极。
ISO 12987:2004 specifies a method for the determination of thermal conductivity of carbonaceous material in the temperature range of 20 °C to 60 °C. The typical range of thermal conductivity for these materials is 2 W/(K·m) to 100 W/(K·m).
This method can be used for other carbon materials, such as graphitized electrodes for other applications.