1.1
This test method covers the measurement of the relative resistance of magnesia grain to hydration.
1.2
The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.
1.3
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
1.4
This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
====== Significance And Use ======
3.1
This test method determines relative hydration resistance of magnesia grain.
3.2
This test method is used in industry to evaluate grain samples and is used for specification purposes in some cases.
3.3
Care must be taken in interpreting the data.